基于LTCC技术的WLAN射频前端的研制  

WLAN RF front-end fabricated using the LTCC technique

在线阅读下载全文

作  者:王莎鸥[1] 尉旭波[1] 李力力[1] 曾志毅[1] 杨邦朝[1] 

机构地区:[1]电子科技大学电子科学与技术学院,四川成都610054

出  处:《电子元件与材料》2010年第12期40-43,共4页Electronic Components And Materials

摘  要:采用低温共烧陶瓷(LTCC)集成技术,设计和制作了具有立体化新型结构的无线局域网(WLAN)射频前端,并对制得的产品模块进行了测试。结果表明:采用LTCC技术制得的WLAN射频前端的外形尺寸仅为29 mm×18 mm×5 mm,远小于传统同类型WLAN射频前端的尺寸。在2.4~2.5 GHz的工作频率范围内,所制WLAN射频前端的最大输出功率为27 dBm,噪声系数小于1.7 dB,接收增益大于15 dB,发射增益大于20 dB。Wireless local area network(WLAN) radio frequency(RF) front-end with 3D structure was designed and fabricated by using the low temperature co-fired ceramic(LTCC) integration technique,and was then tested.The results show that the size of the WLAN RF front-end fabricated using the LTCC technique is only 29 mm × 18 mm × 5 mm and is much smaller than that of conventional WLAN RF front-end.In the frequency range of 2.4~2.5 GHz,the maximum output power of the fabricated WLAN RF front-end is 27 dBm,while its noise figure,receive gain and transmit gain are less than 1.7 dB,more than 15 dB and more than 20 dB,respectively.

关 键 词:低温共烧陶瓷 无线局域网 射频前端 

分 类 号:TM713[电气工程—电力系统及自动化]

 

参考文献:

正在载入数据...

 

二级参考文献:

正在载入数据...

 

耦合文献:

正在载入数据...

 

引证文献:

正在载入数据...

 

二级引证文献:

正在载入数据...

 

同被引文献:

正在载入数据...

 

相关期刊文献:

正在载入数据...

相关的主题
相关的作者对象
相关的机构对象