supported by the National Natural Sciences Foundation of China(50071066)
In this investigation, protective layers were formed on aluminum substrate by Plasma Electrolytic Deposition (PED) using sodium silicate solution. The relation between the thickness of the layer and process time were ...
Project(50071066) supported by the National Natural Science Foundation of China; Project(B41) supported by the Doctoral Foundation of Yanshan University, China; Project(YDJJ: 0169) supported by the Science & Technology Foundation of Yanshan University, China
Composite coatings were obtained on A3 steel by hot dipping aluminum(HDA) at 720 ℃ for 6 min and micro-plasma oxidation(MPO) in alkali electrolyte. The surface morphology, element distribution and interface structure...